Analysis of wood tissues by time-of-flight secondary ion mass spectrometry

  • Elena N. Tokareva , Andrey V. Pranovich , Pedro Fardim , Geoffrey Daniel and Bjarne Holmbom
Published/Copyright: November 1, 2007
Holzforschung
From the journal Volume 61 Issue 6

Abstract

The distribution of lignin, carbohydrates, and metal ions on the surface of spruce and aspen wood tissue sections was investigated by time-of-flight secondary ion mass spectrometry (ToF-SIMS). The distribution patterns of metals and lignin in ray cells, vessels, and fibres were different, whereas carbohydrates were uniformly distributed across the sections of all morphological regions. In spruce sapwood, Ca, Mg, Na, K, Fe locations was more pronounced in the bordered pit tori and inner layer of ray parenchyma cells. Little lignin was detected in these regions. In spruce heartwood, the degree of lignification was low on the surfaces of bordered pit tori; however, Na and K were not detected here. In compression wood from spruce, the locations of p-hydroxyphenyl and guaiacyl units was different in cell wall layers. In aspen sapwood, the main locations of Ca, Mg, Na, K were in lumina of longitudinal parenchyma cells and in pits between vessels and ray cells. Low-intensity signals of the secondary ions assigned to lignin were found in the same morphological regions.


Corresponding author. Laboratory of Wood and Paper Chemistry, Åbo Akademi University, Process Chemistry Centre, Porthansgatan 3, FI-20500 Turku/Åbo, Finland Phone: +358-2-2154987 Fax: +358-2-2154868

Received: 2007-2-7
Accepted: 2007-8-14
Published Online: 2007-11-01
Published in Print: 2007-11-01

©2007 by Walter de Gruyter Berlin New York

Articles in the same Issue

  1. Acknowledgement
  2. Subject index
  3. Contents Volume 61 (2007)
  4. Author index
  5. Species index (scientific names)
  6. Meetings
  7. Improvement of Pinus pinaster Ait elite trees selection by combining near infrared spectroscopy and genetic tools
  8. Direct method for the determination of phenolic hydroxyl groups in pulp
  9. Comparative effect of ozone, chlorine dioxide, and hydrogen peroxide on lignin: Reactions affecting pulp colour in the final bleaching stage
  10. Structural modification of eucalypt pulp lignin in a totally chlorine-free bleaching sequence including a laccase-mediator stage
  11. Analysis of wood tissues by time-of-flight secondary ion mass spectrometry
  12. Isolation and identification of residual chromophores from aged bleached pulp samples
  13. Studies on oxidative modifications of cellulose in the periodate system: Molecular weight distribution and carbonyl group profiles
  14. Lignin-carbohydrate network in wood and pulps: A determinant for reactivity
  15. Cross polarisation/magic angle spinning 13C-NMR spectroscopic studies of cellulose structural changes in hardwood dissolving pulp process
  16. Fungal decay of spruce and beech wood assessed by near-infrared spectroscopy in combination with uni- and multivariate data analysis
  17. Paper mill sludge as a component of wood adhesive formulation
  18. Implementation of sorption hysteresis in multi-Fickian moisture transport
  19. Time/temperature equivalence in the dry wood creep response
  20. Neural network prediction of bending strength and stiffness in western hemlock (Tsuga heterophylla Raf.)
  21. Bending properties of particleboard and MDF layers
  22. Gold as an X-ray CT scanning contrast agent: Effect on the mechanical properties of wood plastic composites
  23. Lignin modification in the initial phase of softwood kraft pulp delignification with polyoxometalates (POMs)
Downloaded on 31.12.2025 from https://www.degruyterbrill.com/document/doi/10.1515/HF.2007.119/pdf
Scroll to top button