Metal-oxide-modified nanostructured carbon application as novel adsorbents for chromate ion removal from water
-
and
Abstract
In the present work, nickel oxide and iron oxide nanoparticles were synthesized inside the pore system of nanoporous carbon and were used as adsorbents to remove hexavalent chromium. The structural order and textural properties of the new carbonaceous adsorbents were studied by X-ray diffraction analysis and nitrogen adsorption. Experiments were conducted in batch mode with the variables such as contact time and solution pH. Adsorption equilibrium was achieved within 3–4 h for initial Cr(VI) of 10–100 mg.L−1. Maximum sorption capacity of Ni–NC and Fe–NC was observed as 0.86 mmol.g−1 and 1.17 mmol.g−1 respectively.
References
[1] Y.C.Sharma, Colloids Surf. A: Physiochem. Eng. Aspects215 (2003) 155. 10.1016/S0927-7757(02)00485-5Search in Google Scholar
[2] Z.Kowalski: J. Hazard. Mater.37 (1994) 137. 10.1016/0304-3894(94)85042-9Search in Google Scholar
[3] US Department of Health and Human Services, Toxicological Profile for Chromium, Public Health Service Agency for Toxic substances and Diseases Registry, Washington, DC1991.Search in Google Scholar
[4] WHO, Guidelines for Drinking-Water Quality, World Health Organization, Geneva1993.Search in Google Scholar
[5] J.W.Patterson: Industrial Wastewater Treatment Technology, second edition, Butterworth, Boston, (1985) 217.Search in Google Scholar
[6] I.L.Lagadic, M.K.Mitchell, B.D.Payne: Environ. Sci. Technol.35 (2001) 984. 10.1021/es001526mSearch in Google Scholar
[7] N.Zhao, N.Wei, J.Li, Z.Qiao, J.Cui, F.He: Chem. Eng. J.115 (2005) 133. 10.1016/j.cej.2005.09.017Search in Google Scholar
[8] C.A.Basar, A.Karagunduz, B.Keskinler: Appl. Surf. Sci.218 (2003) 170. 10.1016/S0169-4332(03)00576-2Search in Google Scholar
[9] R.Ryoo, S.H.Joo, S.Jun: J. Phys. Chem B.103 (1999) 7743. 10.1021/jp991673aSearch in Google Scholar
[10] B.Sakintuna, Y.Yurum: Ind. Eng. Chem. Res.44 (2005) 2893. 10.1021/ie049080wSearch in Google Scholar
[11] W.Tanthapanichakoona, P.Ariyadejwanichb, P.Japthongb, K.Nakagawac, S.R.Mukaic, H.Tamonc: Water Res.39 (2005) 1347. PMid: 15862334; 10.1016/j.watres.2004.12.044Search in Google Scholar
[12] Y.R.Lin, H.Teng: Micropor. Mesopor. Mater.54 (2002) 167. 10.1016/S1387-1811(02)00380-3Search in Google Scholar
[13] V.M.Gun'koW.R.Betz, S.Patel, M.C.Murphy, S.V.Mikhalovsky: Carbon44 (2006) 1258. 10.1016/j.carbon.2005.10.038Search in Google Scholar
[14] Y.Shao, L.Wang, J.Zhang, M.Anpo: Micropor. Mesopor. Mater.109 (2005) 20835.Search in Google Scholar
[15] M.Ghiaci, R.Kia, A.Abbaspur, F.Seyedeyn-Azad: Sep. Purif. Technol.40 (2004) 285. 10.1016/j.seppur.2004.03.009Search in Google Scholar
[16] M.J.Baniamerian, S.E.Moradi, A.Noori, H.Salahi: Appl. Surf. Sci.256 (2009) 1347.Search in Google Scholar
[17] X.W.Wu, H.W.Ma, Y.R.Zhang: Appl. Clay Sci.48 (2010) 538.Search in Google Scholar
[18] D.Zhao, J.Feng, Q.Huo, N.Melosh, G.H.Frederickson, B.F.Chmelka: Science279 (1998) 548. PMid: 9438845; 10.1126/science.279.5350.548Search in Google Scholar
[19] S.Jun, S.H.Joo, R.Ryoo, M.Kruk, M.Jaroniec, Z.Liu, T.Ohsuna, O.Terasaki: J. Am. Chem. Soc.122 (122) (2000) 10712. 10.1021/ja002261eSearch in Google Scholar
[20] H.Li, S.Zhu, H.Xi, R.Wang: Micropor. Mesopor. Mater.89 (2006) 196. 10.1016/j.micromeso.2005.10.033Search in Google Scholar
[21] Z.Gu, J.Fang, B.Deng: Environ. Sci. Technol.39 (2005) 3833. 10.1021/es048179rSearch in Google Scholar
[22] D.Dollimore, G.R.Heal: J. Colloid Interface Sci.33 (1970) 508. 10.1016/0021-9797(70)90002-0Search in Google Scholar
© 2012, Carl Hanser Verlag, München
Articles in the same Issue
- Contents
- Contents
- Original Contributions
- Diffusion characteristics in the Cu–Ti system
- Hydrogen permeability with dislocation in low carbon, aluminium-killed, enamel-grade steels
- Numerical simulation of the evolution of primary and secondary Nb(CN), Ti(CN) and AlN in Nb-microalloyed steel during continuous casting
- Microstructure evolution in a 2618 aluminium alloy during creep-fatigue tests
- Microstructure characterization in the weld joint of a high nickel austenitic alloy and Cr18-Ni8 stainless steel
- The reoptimization of the binary Se–Te system
- Phase diagram of the Sm–Dy–Fe ternary system
- Thermophysical properties of solid phase Ti-6Al-4V alloy over a wide temperature range
- Determination of mechanical properties by nanoindentation in the case of viscous materials
- Mechanical properties and biodegradable behavior of Mg–6%Zn–Ca3(PO4)2 metal matrix composites in Ringer's solution
- Effect of Ti addition on the wettability of Al–B4C metal matrix composites
- Effect of pH on structure, morphology and optical properties of nanosized cupric oxide prepared by a simple hydrolysis method
- Metal-oxide-modified nanostructured carbon application as novel adsorbents for chromate ion removal from water
- Biological evaluation of micro-nanoporous layer on Ti–Ag alloy for dental implant
- Design of damage tolerance in high-strength steels
- Creep modeling and creep life estimation of Gr.91
- Influence of the layer architecture of DLC coatings on their wear and corrosion resistance
- Potential of mechanical surface treatment for mould and die production
- Short Communications
- Discussion of defect analysis of a Ti-6Al-4V alloy forging ring
- DGM News
- DGM News
Articles in the same Issue
- Contents
- Contents
- Original Contributions
- Diffusion characteristics in the Cu–Ti system
- Hydrogen permeability with dislocation in low carbon, aluminium-killed, enamel-grade steels
- Numerical simulation of the evolution of primary and secondary Nb(CN), Ti(CN) and AlN in Nb-microalloyed steel during continuous casting
- Microstructure evolution in a 2618 aluminium alloy during creep-fatigue tests
- Microstructure characterization in the weld joint of a high nickel austenitic alloy and Cr18-Ni8 stainless steel
- The reoptimization of the binary Se–Te system
- Phase diagram of the Sm–Dy–Fe ternary system
- Thermophysical properties of solid phase Ti-6Al-4V alloy over a wide temperature range
- Determination of mechanical properties by nanoindentation in the case of viscous materials
- Mechanical properties and biodegradable behavior of Mg–6%Zn–Ca3(PO4)2 metal matrix composites in Ringer's solution
- Effect of Ti addition on the wettability of Al–B4C metal matrix composites
- Effect of pH on structure, morphology and optical properties of nanosized cupric oxide prepared by a simple hydrolysis method
- Metal-oxide-modified nanostructured carbon application as novel adsorbents for chromate ion removal from water
- Biological evaluation of micro-nanoporous layer on Ti–Ag alloy for dental implant
- Design of damage tolerance in high-strength steels
- Creep modeling and creep life estimation of Gr.91
- Influence of the layer architecture of DLC coatings on their wear and corrosion resistance
- Potential of mechanical surface treatment for mould and die production
- Short Communications
- Discussion of defect analysis of a Ti-6Al-4V alloy forging ring
- DGM News
- DGM News