Article
Licensed
Unlicensed
Requires Authentication
Degradation of polyethylene glycol and hemicellulose in the Vasa
-
Gunnar Almkvist
and Ingmar Persson
Published/Copyright:
December 5, 2007
Abstract
Mass spectrometric analysis of aqueous wood extracts from the Swedish warship Vasa reveals a serious chemical condition in the depth of the wood. The surface is less affected. Polyethylene glycol, used as conservation agent, is affected and partly degraded, and low-molecular fragments from hemicellulose are found at sites with high iron content and low pH. These findings imply a catalytic oxidative process and acidic hydrolysis in the wood, which contributes to a new picture of the challenge of long-term preservation of the Vasa.
Keywords: catalytic oxidation; hemicelluloses; hydrolysis; matrix-assisted laser desorption/ionization-time of flight (MALDI-TOF); polyethylene glycol; Vasa; wood degradation
Received: 2007-3-21
Accepted: 2007-10-1
Published Online: 2007-12-05
Published in Print: 2008-1-1
©2008 by Walter de Gruyter Berlin New York
You are currently not able to access this content.
You are currently not able to access this content.
Articles in the same Issue
- Meetings
- Evaluation of Eucalyptus grandis Hill ex Maiden biopulping with Ceriporiopsis subvermispora under non-aseptic conditions
- Paper dry strength improvement by xyloglucan addition: Wet-end application, spray coating and synergism with borate
- A new and facile method for isolation of lignin from wood based on complete wood dissolution
- Isolation and characterization of lignins from Eucalyptus grandis Hill ex Maiden and Eucalyptus globulus Labill. by enzymatic mild acidolysis (EMAL)
- Fractionation and characterization of xylan rich extracts from birch
- Polyoxometalate (POM) oxidation of lignin model compounds
- Pyrolytic cleavage mechanisms of lignin-ether linkages: A study on p-substituted dimers and trimers
- Polysaccharide degradation in waterlogged oak wood from the ancient warship Vasa
- Degradation of polyethylene glycol and hemicellulose in the Vasa
- Selection criteria of Eucalyptus globulus Labill. for production of chemithermomechanical pulps (CTMP)
- The effect of (induced) dislocations on the tensile properties of individual Norway spruce fibres
- Mode I and Mode II fracture toughness of densified Sitka spruce fabricated in an airtight atmosphere with high-temperature steam
- Characteristic properties of embedding strength for the nailing of the gonfolo rose (Qualea rosea Aubl.)
- Adhesive penetration of wood cell walls investigated by scanning thermal microscopy (SThM)
- Laboratory screening of tropical hardwoods for natural resistance to the marine borer Limnoria quadripunctata: The role of leachable and non-leachable factors
- Decay resistance of wood treated with amino-silicone compounds
- Hydrothermal treatment of mixed preservative-treated wood waste
- Variation of tracheid length within annual rings of Scots pine and Norway spruce
Keywords for this article
catalytic oxidation;
hemicelluloses;
hydrolysis;
matrix-assisted laser desorption/ionization-time of flight (MALDI-TOF);
polyethylene glycol;
Vasa;
wood degradation
Articles in the same Issue
- Meetings
- Evaluation of Eucalyptus grandis Hill ex Maiden biopulping with Ceriporiopsis subvermispora under non-aseptic conditions
- Paper dry strength improvement by xyloglucan addition: Wet-end application, spray coating and synergism with borate
- A new and facile method for isolation of lignin from wood based on complete wood dissolution
- Isolation and characterization of lignins from Eucalyptus grandis Hill ex Maiden and Eucalyptus globulus Labill. by enzymatic mild acidolysis (EMAL)
- Fractionation and characterization of xylan rich extracts from birch
- Polyoxometalate (POM) oxidation of lignin model compounds
- Pyrolytic cleavage mechanisms of lignin-ether linkages: A study on p-substituted dimers and trimers
- Polysaccharide degradation in waterlogged oak wood from the ancient warship Vasa
- Degradation of polyethylene glycol and hemicellulose in the Vasa
- Selection criteria of Eucalyptus globulus Labill. for production of chemithermomechanical pulps (CTMP)
- The effect of (induced) dislocations on the tensile properties of individual Norway spruce fibres
- Mode I and Mode II fracture toughness of densified Sitka spruce fabricated in an airtight atmosphere with high-temperature steam
- Characteristic properties of embedding strength for the nailing of the gonfolo rose (Qualea rosea Aubl.)
- Adhesive penetration of wood cell walls investigated by scanning thermal microscopy (SThM)
- Laboratory screening of tropical hardwoods for natural resistance to the marine borer Limnoria quadripunctata: The role of leachable and non-leachable factors
- Decay resistance of wood treated with amino-silicone compounds
- Hydrothermal treatment of mixed preservative-treated wood waste
- Variation of tracheid length within annual rings of Scots pine and Norway spruce