Abstract

Cadmium electrodeposited EN24 steel shear bolts were used in space programme. Recently, one of five bolts subjected to wedge test at 18 Nm torque encountered failure. Fracture surface of failed bolt had two distinct regions, when viewed under scanning electron microscope. Outer region consisted of brittle features while inner region had ductile failure. Detailed investigation revealed that the bolt failure was due to hydrogen embrittlement. Electro-deposition of cadmium was main source for hydrogen entrapment, which could not be compelled out by post plating baking treatment.

Kurzfassung

In einem Raumfahrtprogramm kamen elektrolytisch mit Cadmium beschichtete Scherbolzen aus EN24-Stahl zum Einsatz. Unlängst versagte einer der fünf Bolzen bei einem Keiltest bei einem Drehmoment von 18 Nm. Die Bruchfläche des entsprechenden Bolzens wies bei Betrachtung unter dem Rasterelektronenmikroskop zwei unterschiedliche Bereiche auf. Der äußere Bereich hatte Merkmale eines spröden Versagens, während der innere Bereich einen Verformungsbruch aufwies. Eine eingehende Untersuchung zeigte, dass der Bolzen aufgrund von Wasserstoffversprödung versagte. Die elektrolytische Abscheidung von Cadmium war Hauptgrundlage für die Ansammlung von Wasserstoff. Dieser konnte durch die nach dem Beschichten erfolgende Wärmebehandlung im Ofen nicht aus dem Werkstoff herausgetrieben werden.


Übersetzung: E. Engert


References / Literatur

1. Metals hand book, 9th edition, vol. 13, corrosion, ASM International, 1987, p. 427.Search in Google Scholar

2. John A.Fellows, editor, Metals Hand Book, 8th edition, vol. 9, Fractography and Atlas of Fractographs, ASM, Metals Park, Ohio, 1974, p. 111Search in Google Scholar

3. Carter, T.J; Cornish, L.A.: Hydrogen in metals, Eng. Fail. Anal.8, 113121 (2001) DOI: 10.1016/S1350-6307(99)00040-0Search in Google Scholar

4. Howard E.Boyer, editor, Metals hand Book, 8th edition, vol. 10, Failure Analysis and Prevention, American Society for Metals, Metals park, Ohio, 1975, p. 230Search in Google Scholar

5. ASTM International, B850-90 (reapproved 2004) standard guide for post-coating treatment of steel for reducing risk of hydrogen embrittlement.Search in Google Scholar

6. JhaA.K.; Narayanan, P.R.; Sreekumar, K.; Mittal, M.N.; Ninan, K.N.: Eng. Fail. Anal.15, 431439 (2008) DOI: 10.1016/j.engfailanal.2007.05.008Search in Google Scholar

7. Jha AbhayK.; Sreekumar, J.: Fail. Anal. and Preven. (2009) 9:42042810.1007/s11668-009-9277-3Search in Google Scholar

Received: 2013-09-26
Accepted: 2014-03-21
Published Online: 2014-07-14
Published in Print: 2014-07-14

© 2014, Carl Hanser Verlag, München

Downloaded on 3.11.2025 from https://www.degruyterbrill.com/document/doi/10.3139/147.110268/html
Scroll to top button