Home Technology The anisotropy of deformation for friction stir processed Mg alloy due to the existence of onion rings
Article
Licensed
Unlicensed Requires Authentication

The anisotropy of deformation for friction stir processed Mg alloy due to the existence of onion rings

  • Du Xinghao and Wu Baolin
Published/Copyright: March 1, 2013

Abstract

In the present study, it is found that one-pass friction stir processed AZ61 alloy exhibits inferior deformation ability along the longitudinal direction compared with the transverse direction at high temperatures. Based on observation of microstructure and fracture surface, premature onion ring splitting is suggested to be mainly responsible for this anisotropy of deformation behavior. Furthermore, the homogeneous microstructure from multi-pass friction stir processing can cure the premature onion ring splitting and then exhibit isotropic high-temperature superplastic deformation behavior.


2 Correspondence address: Prof. Wu Baolin, Department of Materials Engineering, Shenyang Institute of Aeronautical Engineering, Shenyang, 110034, PRC, Tel.: +86 24 86 141 696. E-mail:

References

[1] W.M.Thomas, E.D.Nicholas, J.C.Needham, M.G.Church, P.Templesmith, C.J.Dawes: The Welding Institute, TWI, International Patent Application No. PCT/GB92/02203 and GB Patent Application No. 9125978.81991.Search in Google Scholar

[2] R.S.Mishra, M.W.Mahoney, S.X.McFadden, N.A.Mara, A.K.Mukherjee: Scripta Mater.42(2000)163.10.1016/S1359-6462(99)00329-2Search in Google Scholar

[3] K.Colligan: Weld. Res.65(1999)229.Search in Google Scholar

[4] K.N.Krishman: Mater. Sci. Eng. A327(2002)246.10.1016/S0921-5093(01)01474-5Search in Google Scholar

[5] G.Biallas: Mechanical Properties and corrosion behaviour of friction stir welded 2024-T6, First International Conference on Friction Stir Welds, Thousand Oaks, CA(1999).Search in Google Scholar

[6] P.L.Threadgill: Friction Stir Welding – State of the art, TWI report(1999)678.Search in Google Scholar

[7] H.Larsson, L.Karlsson, S.Stoltz, E.-L.Bergqvist: Joining of dissimilar Al-alloys by Friction Stir Welding, Second International Conference on Friction Stir Welds, Gothenburg, Sweden, 2000.Search in Google Scholar

[8] B.Yang, J.Yan, M.A.Suttion, A.P.Reynolds: Mater. Sci. Eng. A364(2004)55.10.1016/S0921-5093(03)00532-XSearch in Google Scholar

[9] Z.Y.Ma, S.R.Sharma, R.S.Mishra: Scripta Mater.54(2006)1623.10.1016/j.scriptamat.2006.01.010Search in Google Scholar

[10] Z.Y.Ma, R.S.Mishra, M.W.Manohey, R.Grimes: Mater. Sci. Eng. A351(2003)148.10.1016/S0921-5093(02)00824-9Search in Google Scholar

[11] I.Charit, R.S.Mishra, Mater. Sci. Eng. A359(2003)290.10.1016/S0921-5093(03)00367-8Search in Google Scholar

[12] I.Charit, Z.Y.Ma, R.S.Mishra, in: Z.Jin, A.Beaudoin, T.A.Bieler, B.Radhakrishnan (Eds.), Hot Deformation of Aluminum Alloys III, TMS(2003)331.Search in Google Scholar

[13] A.W.Bowen: Mater. Sci. Technol.6(1990)1058.10.1179/026708390790190045Search in Google Scholar

[14] Z.Y.Ma, R.S.Mishra, M.W.Mahoney: Scripta Mater.50(2004)931.10.1016/j.scriptamat.2004.01.012Search in Google Scholar

[15] A.H.Feng, Z.Y.Ma: Scripta Mater.56(2007)397.10.1016/j.scriptamat.2006.10.035Search in Google Scholar

[16] P.Cavaliere, P.P.De Marco: J. Mater. Proc. Tech.184(2007)77.10.1016/j.jmatprotec.2006.11.005Search in Google Scholar

[17] Z.Y.Ma, R.S.Mishra, M.W.Mahoney: Acta Mater.50(2002)4419.10.1016/S1359-6454(02)00278-1Search in Google Scholar

[18] P.Cavaliere, A.Squillace: Materials Characterization2(2005)136.10.1016/j.matchar.2005.04.007Search in Google Scholar

[19] T.G.Nieh, J.Wadsworth: Int. Mater. Rev.44(1999)59.10.1179/095066099101528225Search in Google Scholar

[20] D.H.Bae, A.K.Ghosh: Acta Mater.50(2002)511.10.1016/S1359-6454(01)00375-5Search in Google Scholar

[21] A.K.Ghosh, D.H.Bae, S.L.Semiatin: Mater. Sci. Forum.304(1999)609.10.4028/www.scientific.net/MSF.304-306.609Search in Google Scholar

[22] W.J.Arbegast, in: Z.Jin, A.Beaudoin, T.A.Bieler, B.Radhakrishnan (Eds.), Hot Deformation of Aluminum Alloys III, TMS(2003)313.Search in Google Scholar

Received: 2007-04-11
Accepted: 2007-10-23
Published Online: 2013-03-01
Published in Print: 2008-02-01

© 2008, Carl Hanser Verlag, Munich

Downloaded on 24.12.2025 from https://www.degruyterbrill.com/document/doi/10.3139/146.101615/html?lang=en
Scroll to top button