Comparison of lightweight Japanese tissues for overall stabilization of documents damaged by iron gall ink corrosion and an alternative to silk screen frames
-
Andrea Pataki-Hundt
Andrea Pataki-Hundt is professor at the Cologne Institute for Conservation Sciences (CICS) since 2017 at the TH Köln. She has been research assistant (1998–2017) of the conservation laboratory at the programme for conservation of works of art on paper, archive- and library materials at the State Academy of Art and Design Stuttgart, where she also obtained her diploma (1997) and her PhD (2005).Cosima Walter is a Master student in the programme for conservation of works of art on paper, archival- and library material at the State Academy of Art and Design in Stuttgart. This paper is based on her Bachelor thesis.and Cosima Walter
Abstract
Paper documents with severe iron gall ink corrosion are difficult to handle. While a defined treatment for the chemical stabilisation exists already, methods to improve the mechanical stabilisation have yet to be developed. The degradation of the selected objects was so advanced that the documents needed special attention concerning handling and mechanical re-enforcement. After a calciumphytate-calciumhydrogen treatment, documents were lined with light weight Japanese paper and gelatine. A workflow for treating severely degraded iron gall ink documents was developed. Since the removal of objects from the silk screen frames after the wet treatment proved to be too difficult, a PE-board was introduced as an alternative washing support. Most synthetic fleeces such as Hollytex or Paraprint adhere to its granulated surface by mechanical means. This makes PE-board a practical support during any wet treatment of paper-based objects.
Zusammenfassung
Vergleich von dünnen Japanpapieren für die flächige Kaschierung von tintenfraßgeschädigten Dokumenten und eine Alternative zu konventionellen Siebrahmen.
Papierdokumente mit Tintenfraß, welche der Zustandsklasse vier gemäß Reißland und Hofenk de Graaff zugeordnet wurden, sind mechanisch fragil und schwer zu handhaben. Für diese Objekte gibt bereits eine definierte Behandlung zur chemischen Stabilisierung. Dieser Beitrag beschäftigt sich mit einer weiteren Verfeinerung der Techniken zur Handhabung während der wässrigen Behandlung und mit Stabilisierungstechniken für eine flächige Kaschierung von schwer geschädigten Tintenfraßobjekten. Die Schädigung der ausgewählten Objekte ist so weit fortgeschritten, dass sie besondere Aufmerksamkeit bei der Handhabung und bei der mechanischen Stabilisierung benötigten. Die Calciumphytat/ Calciumhydrogencarbonatbehandlung mit einer nachfolgenden Kaschierung mit dünnen Japanpapier und Gelatine wurde eingesetzt. Aufgrund ihrer Fragilität wurden die Dokumente zwischen zwei Paraprint OL Vliesen wässrig behandelt. Nach dem Kaschieren wurden die Objekte kurz eingepresst, um eine gute Haftung zwischen originalem Papier und dem Japanpapier zu gewährleisten. Auf dieser Grundlage wurde ein Arbeitsablauf entwickelt, um ein kleines Konvolut schwer geschädigter Dokumente mit Eisengallustinte zu behandeln. Da das Entfernen der Objekte aus dem zunächst verwendeten Siebrahmen sehr schwer war, wird in diesem Beitrag eine alternative Arbeitshilfe vorgestellt. Eine PE-Platte eignet sich perfekt als Unterstützung, um die nassen Objekte zu bewegen und könnte die konventionellen Siebrahmen ersetzten. Die meisten synthetischen Vliese wie Hollytex® und Paraprint haften mechanisch auf der gekörnten Oberfläche. Die PE-Platte ist nicht nur für die Behandlung von durch Tintenfraß geschädigte Objekte interessant, sondern auch für andere wässrige Behandlungen geeignet.
Resumé
La stabilisation d’ensemble des documents corrodés par de l’encre métallo-gallique et une alternative au cadre écran de soie: le cadre de PE
Les documents papier présentant une corrosion de l’encre métallo-gallique de niveau 4 sont difficiles à manipuler. Il existe déjà un traitement défini pour la stabilisation chimique mais pas pour la stabilisation mécanique. La détérioration des objets choisis étaient tellement avancée qu’une attention particulière était nécessaire pour leur manipulation et pour leur renforcement mécanique. La méthode au phytate et à l’hydrogène de calcium a été appliquée avec un doublage ultérieur avec un papier japon de fin grammage et de la gélatine. Cette procédure a été rendue possible par l’utilisation de Paraprint OL60 et d’une étape de contact par pression.
Un flux de travail pour traiter un petit groupe de documents fortement dégradés par l’encre métallo-gallique a été développé. La délamination des objets en dehors des cadres écran de soie devint trop difficile et il a été nécessaire d’introduire un support de lavage alternatif. Le cadre de PE représente le support technique idéal pour pouvoir manipuler le sandwich avec l’objet mouillé et il a pu remplacer le cadre écran de soie. Grâce à leur surface rugueuse, la plupart des non tissés synthétiques comme le hollitex® ou le paraprint adhèrent grâce à des forces mécaniques. Le cadre de PE n’est pas seulement intéressant pour traiter des documents à l’encre métallo-gallique mais il est aussi adapté pour tout lavage avec support.
About the author
Andrea Pataki-Hundt is professor at the Cologne Institute for Conservation Sciences (CICS) since 2017 at the TH Köln. She has been research assistant (1998–2017) of the conservation laboratory at the programme for conservation of works of art on paper, archive- and library materials at the State Academy of Art and Design Stuttgart, where she also obtained her diploma (1997) and her PhD (2005).Cosima Walter is a Master student in the programme for conservation of works of art on paper, archival- and library material at the State Academy of Art and Design in Stuttgart. This paper is based on her Bachelor thesis.
Acknowledgements
We would like to thank Günther Müller, in charge of the conservation of the burnt papers of the Herzogin Anna Amalia Bibliothek in Weimar, for his kind guidance on the short contact pressure method.
References
Banik, G.: Phänomene und Ursachen von Tintenfraß auf Papier-eine Einführung. In: Tintenfraßschäden und ihre Behandlung. B. G. Banik and H. Weber (eds.), Stuttgart: Kohlhammer, 1999: 13–24.Search in Google Scholar
Bansa, H., Ishii, R.: What fiber for paper strengthening?. Restaurator 20 (1999): 198–224.10.1515/rest.1999.20.3-4.198Search in Google Scholar
Desroches, M., Duplat, V., Rouchon, V.: Instructables: An aqueous treatment for highly damaged manuscripts: Minimising the risk of mechanical damage. Journal of Paper Conservation 13 (2012): 36–37.10.1080/20571682.2012.12462143Search in Google Scholar
Henniges, U., Potthast, A.: Phytate treatment of metallo-gallate inks: Investigation of its effectiveness on model and historic paper samples. Restaurator 29 (2008): 219–234.10.1515/rest.2008.016Search in Google Scholar
Huhsmann, E., Hähner, U.: Application of the Non-woven Viscose Fabric Paraprint OL 60 for Float Sreen Washing of Documents Damaged by Iron Gall Ink Corrosion. Restaurator 28 (2007): 140–151.10.1515/REST.2007.140Search in Google Scholar
Huhsmann, E., Hähner, U.: Work standard for the treatment of 18th–19th-century iron gall ink documents with calcium phytate and calcium hydrogen carbonate. Restaurator 29 (2008): 274–319.10.1515/rest.2008.020Search in Google Scholar
Kirchner, S.: Kapillarreinigung, eine schonende Methode der Feuchtreinigung in der Papierrestaurierung. PapierRestaurierung 2, Suppl. (2001): 73–80.10.1080/15632628.2001.12461763Search in Google Scholar
Kolbe, G.: Gelatine in historic paper production and as inhibiting agent for iron-gall ink corrosion on paper. Restaurator 25 (2004): 26–39.10.1515/REST.2004.26Search in Google Scholar
Martin, A., Rouchon, V., Aubry, T., Cauliez, N., Deroches, M., Margesz, M.: Local strengthening of mold-damaged manuscripts. Journal of Paper Conservation 12 (2011): 21–29.Search in Google Scholar
Müller, G.: Zur implantierten Gesamtstabilisierung von Tintenfraß auf Papiergrundlage. In: Tintenfraßschäden und ihre Behandlung, G. Banik and H. Weber (eds), Stuttgart: W. Kohlhammer, 1999: 278–283.Search in Google Scholar
Müller, G.: Die Weimarer Aschebücher. In: Restaurieren nach dem Brand. B. J. Weber and U. Hähner (eds), Weimar: Michael Imhof Verlag, 2014: 132–138.Search in Google Scholar
Neevel, J. G.: Application issues of the bathophenanthroline test for iron (II) Ions. Restaurator 30 (2000): 3–15.10.1515/rest.002Search in Google Scholar
Pataki, A.: Remoistenable tissue preparation and its practical aspects. Restaurator 29 (2009): 1–19.10.1515/rest.004Search in Google Scholar
Reissland, B., Hofenk De Graaff, J.: Condition rating for paper with iron gall ink, Instituut Collectie Nederland (ICN), ICN Information (2000): 1–4.Search in Google Scholar
Rouchon, V., Desroches, M., Duplat, V., Letouzey, M., Stordiau-Pallot, J.: Methods of aqueous treatments: The last resort for badly damaged iron gall in manuscripts. Journal of Paper Conservation 13 (2012): 7–13.10.1080/20571682.2012.12462140Search in Google Scholar
Schönbohm, D., Blüher, A., Banik, G.: Enzymes in solvent conditioned poultices for the removal of starch-based adhesives from iron gall ink corroded manuscripts. Restaurator 25 (2004): 267–281.10.1515/REST.2004.267Search in Google Scholar
Seger, A.: Bakteriencellulose - Einsatzmöglichkeiten in der Papierrestaurierung. Arbeitsblätter Der NRW-Papierrestauratoren 21 (2013): 65–71.Search in Google Scholar
Seger, A.: Bakteriencellulose für die Pergamentrestaurierung. BC-Tissue-ein neues Material in der Anwendung. Arbeitsblätter Der NRW-Papierrestauratoren 22 (2016): 43–48.Search in Google Scholar
Sistach, M., Marin, E., Garcia, J.: Evaluation of alkaline compounds used for deacidification and simultaneous lining of extremely degraded manuscripts. Restaurator 38 (2017): 249–272.10.1515/res-2016-0034Search in Google Scholar
Titus, S., Schneller, R., Huhsmann, E., Hähner, U., Banik, G.: Stabilising local areas of loss in iron gall ink copy documents from the Savigny estate. Restaurator 30 (2009): 16–50.10.1515/rest.003Search in Google Scholar
Walter, C.: Einbettverfahren für Tintenfraß geschädigtes Schriftgut, Vergleich verschiedener Japanpapiere und Kaschiermethoden, Bachelorthesis, unpublished graduate thesis, State Academy of Art and Design Stuttgart, 2016.Search in Google Scholar
© 2018 Walter de Gruyter GmbH, Berlin/Boston
Articles in the same Issue
- Frontmatter
- Composition and source of white precipitations on the inner side of papyrus glazings
- Comparison of lightweight Japanese tissues for overall stabilization of documents damaged by iron gall ink corrosion and an alternative to silk screen frames
- Blu-Ray Media Stability and Suitability for Long-Term Storage
Articles in the same Issue
- Frontmatter
- Composition and source of white precipitations on the inner side of papyrus glazings
- Comparison of lightweight Japanese tissues for overall stabilization of documents damaged by iron gall ink corrosion and an alternative to silk screen frames
- Blu-Ray Media Stability and Suitability for Long-Term Storage