Size exclusion chromatographic and UV-VIS absorption analyses of unbleached and bleached softwood kraft pulps using LiCl/1,3-dimethyl-2-imidazolidinone as a solvent
-
Masahiro Yanagisawa
Abstract
Unbleached and bleached kraft pulps and holocellulose prepared from softwood were totally soluble in 8% LiCl/1,3-dimethyl-2-imidazolidinone (LiCl/DMI). The solutions were analyzed by size exclusion chromatography with photodiode array and multi-angle laser light scattering detection (SEC-PDA-MALLS). The mobile phase consisted of 1% LiCl/DMI. The degree of polymerization (DP) and DP distribution of the softwood kraft pulps were determined, as well as the DP distribution of residual lignins based on their UV-VIS absorption patterns. Changes in DP for kraft pulps after a conventional bleaching sequence were evaluated, and the residual lignins were analyzed in the same way. Approximately half of the residual lignin in unbleached and bleached kraft pulps was present in polysaccharide fractions with high DP, which represented approximately 90% of the total yield. Some characteristic differences in the UV-VIS absorption pattern were observed between kraft pulps bleached with oxygen and chlorine. DP, DP distribution of polysaccharides, and distribution of residual lignin were clearly different for unbleached kraft pulp, unbleached sulfite pulp, and holocellulose. An unbleached kraft pulp prepared from hardwood showed different properties to the corresponding softwood preparation. The UV-VIS absorption patterns due to residual lignins were also very characteristic for the various pulps and holocellulose.
©2007 by Walter de Gruyter Berlin New York
Articles in the same Issue
- To all readers, authors and subscribers
- Vapor-phase diethyl oxalate pretreatment of wood chips: Part 1. Energy savings and improved pulps
- Vapor-phase diethyl oxalate pretreatment of wood chips: Part 2. Release of hemicellulosic carbohydrates
- Size exclusion chromatographic and UV-VIS absorption analyses of unbleached and bleached softwood kraft pulps using LiCl/1,3-dimethyl-2-imidazolidinone as a solvent
- A new method for the titration of free phenolic groups in pulps
- Adsorption of water-soluble organic dyes on ferrofluid-modified sawdust
- Mechanical properties and creep behavior of lyocell fibers by nanoindentation and nano-tensile testing
- Deformation behavior of wet lignocellulosic fibers
- Changes in physical, mechanical and chemical properties of wood during sterilisation by gamma radiation
- Penetration of poly(ethylene glycol) into wood cell walls of red pine
- Transverse mechanical behaviour and moisture absorption of waterlogged archaeological wood from the Vasa ship
- Determination of residual stress in bonded wood components
- Decohesion of glue bonds in wood connections
- Delamination assessment after drilling medium-density fibreboard (MDF) by digital image analysis
- Effects of thinning and fertilisation on tracheid dimensions and lignin content of Norway spruce
- Detection of β-1-4-galactan in compression wood of Sitka spruce [Picea sitchensis (Bong.) Carrière] by immunofluorescence
- Laboratory and outdoor water repellency and dimensional stability of southern pine sapwood treated with a waterborne water repellent made from resin acids
- Evidence of fungicidal and termicidal properties of Prunus africana heartwood extractives
- The effectiveness of silica treatments against wood-boring invertebrates
- Sap-staining fungi from logs and boards of two commercially important pines in Korea
- Improved quantitative determination of benzalkonium chloride in treated wood by liquid chromatography
- Obituary Anders Björkman (1920–2006)
Articles in the same Issue
- To all readers, authors and subscribers
- Vapor-phase diethyl oxalate pretreatment of wood chips: Part 1. Energy savings and improved pulps
- Vapor-phase diethyl oxalate pretreatment of wood chips: Part 2. Release of hemicellulosic carbohydrates
- Size exclusion chromatographic and UV-VIS absorption analyses of unbleached and bleached softwood kraft pulps using LiCl/1,3-dimethyl-2-imidazolidinone as a solvent
- A new method for the titration of free phenolic groups in pulps
- Adsorption of water-soluble organic dyes on ferrofluid-modified sawdust
- Mechanical properties and creep behavior of lyocell fibers by nanoindentation and nano-tensile testing
- Deformation behavior of wet lignocellulosic fibers
- Changes in physical, mechanical and chemical properties of wood during sterilisation by gamma radiation
- Penetration of poly(ethylene glycol) into wood cell walls of red pine
- Transverse mechanical behaviour and moisture absorption of waterlogged archaeological wood from the Vasa ship
- Determination of residual stress in bonded wood components
- Decohesion of glue bonds in wood connections
- Delamination assessment after drilling medium-density fibreboard (MDF) by digital image analysis
- Effects of thinning and fertilisation on tracheid dimensions and lignin content of Norway spruce
- Detection of β-1-4-galactan in compression wood of Sitka spruce [Picea sitchensis (Bong.) Carrière] by immunofluorescence
- Laboratory and outdoor water repellency and dimensional stability of southern pine sapwood treated with a waterborne water repellent made from resin acids
- Evidence of fungicidal and termicidal properties of Prunus africana heartwood extractives
- The effectiveness of silica treatments against wood-boring invertebrates
- Sap-staining fungi from logs and boards of two commercially important pines in Korea
- Improved quantitative determination of benzalkonium chloride in treated wood by liquid chromatography
- Obituary Anders Björkman (1920–2006)