Summary

The mechanical properties of wood are highly related to its structure, and knowledge regarding the influence of, for instance, density and fiber wall structure is needed for a better utilisation of the wood material. In this work, the Iosipescu method was used to test wood in rolling shear in order to establish the intra-ring variations in the wet shear modulus of spruce wood. The shear modulus increased from the earlywood to the latewood within the annual rings. This increase in the wet shear modulus was explained to 80% by the variations in the density of the wood.

:
Published Online: 2005-06-01
Published in Print: 2001-09-19

Copyright © 2001 by Walter de Gruyter GmbH & Co. KG

Articles in the same Issue

  1. The Influence of Rays on the Transverse Elastic Anisotropy in Green Wood of Deciduous Trees
  2. The Effect of Varying Latewood Proportion on the Radial Distribution of Lignin Content in a Pine Stem
  3. Effects of Environmental Factors on the Color of Sugi (Cryptomeria japonica D. Don) Yellowish Heartwood
  4. Influence of Tannin-Copper Complexes as Preservatives for Wood on Mechanism of Decomposition by Brown-Rot Fungus Fomitopsis palustris
  5. Characteristics of Sludges Produced by Destabilization of CCA Preservative Solutions
  6. Extractives and Structural Components in Wood and Bark of Endemic Oak Quercus vulcanica Boiss
  7. Fragmentation of Suberin and Composition of Aliphatic Monomers Released by Methanolysis of Cork from Quercus suber L.,Analysed by GC-MS, SEC and MALDI-MS
  8. Controlled Assembly of Glucuronoxylans onto Cellulose Fibres
  9. Solid State NMR Studies on Inhomogeneous Structure of Fibre Wall in Kraft Pulp
  10. Characterizing the Surface Roughness of Thermomechanical Pulp Fibers with Atomic Force Microscopy
  11. Thermal Decomposition of Cellulose Crystallites in Wood
  12. Damage and Fracture Mechanisms during Mode I and III Loading of Wood
  13. Directional Characteristics of Near Infrared Light Reflected from Wood
  14. An Investigation of Selected Factors that Influence Hardwood Wettability
  15. Intra-Ring Variations in the Rolling Shear Modulus of Spruce Wood
  16. Study on Alkali-Accessible Chromophores from Unbleached Kraft Pulp
  17. Addition of Boron Based Compound in the LVL Glueline: Effect on the Mechanical Properties and the Leaching of Boron
Downloaded on 16.9.2025 from https://www.degruyterbrill.com/document/doi/10.1515/HF.2001.088/html
Scroll to top button